www婷婷com丨国产免费最爽的乱淫视频a丨精品视频久久久久久丨国产91久久久丨精品一区二区三区在线播放视频丨亚洲国产成人91精品丨亚洲午夜av久久久精品影院色戒丨亚洲精品v日韩精品丨免费在线不卡av丨福利100合集 在线播放丨新天堂网丨国产xxxxx丨久久国产精品成人免费丨激情欧美成人久久综合丨曰本女人牲交全视频播放丨在线亚洲欧美日韩精品专区丨久久国产精品一区二区丨日本另类αv欧美另类aⅴ丨99在线观看精品丨精品无码国产一区二区三区51安丨91精品视频网丨www黄色片丨高清av网址丨日产亚洲一区二区三区丨99成人国产综合久久精品

ZJ-402
Two component polyurethane structural adhesive

ZJ-402 is a two component polyurethane adhesive that, after curing, forms an elastomer with excellent properties such as high strength, aging resistance, vibration fatigue resistance, and low temperature corrosion resistance. ZJ-402 has excellent flame retardant performance, meets the requirements of low odor and low VOC emissions, and complies with EU ROHS regulations. ZJ-402 is suitable for machine dispensing and manual mixing operations; Suitable for bonding various materials such as metal, plastic, rubber, polyester, etc. ZJ-402 is used for bonding between new energy battery module cells and bottom shells, cells and cells, as well as for self bonding or mutual bonding of materials such as metals, ceramics, cement, wood, PU, glass, and fiberglass.

Product features

Smooth gluing and easy construction

Good thixotropy, no flowing

High adhesive strength and wide adaptability of substrate

Excellent aging performance

Flame retardant V-0

Product parameters
Main parameters of ZJ-402
Before curing Unit Typical value Test method
Appearance

A: White paste

B: Blue paste

Visualization
Density

g/cm3

A: 1.33 ± 0.05
B: 1.51 ± 0.05

Cure: 1.42 ± 0.05

GB/T 533-2008

Viscosity

cps

A: 60,000~120,000
B: 60,000~120,000

GB/T 2794-2013, 10 rpm

Mixing ratio

v/v

1:1

Surface drying time

min

> 30

GB/T 13477.5-2002

Complete curing time

d

≤ 7

Hardness

Shore-D

60 ± 5

GB/T 531.1-2008

Thermal conductivity

W/m.k

0.6

ASTM D5470-2017

Volume resistivity

ohm.cm

≥ 1*10^12

GB/T 1410-2006

Flame retardancy

V-0

UL94

Body tensile strength

MPa

≥ 10

GB/T 528-2009

Elongation at break

%

≥ 100

GB/T 528-2009

Tensile shear strength

MPa

≥ 10 (Al–Al)

GB/T 7124-2008

The data in the table is for reference only, please refer to the measured data
Operation and Safety
  • usage method:
  • ? Surface cleaning
  • Use gauze or other tools to remove dust, loose materials, oil stains, and surface water stains from the surface of the area that needs to be coated. If there is rust on the area that needs to be coated with glue, first remove it with a metal brush, and then wipe the surface with acetone and alcohol.
  • Primer and cleaning agent
  • To achieve optimal adhesion performance, corresponding primers and cleaning agents should be used. When applying primer and cleaning agent, it should be ensured that the application is uniform and there is no accumulation of primer or cleaning agent or the surface of the substrate is not covered.
  • ? Mixing
  • ZJ-402 two-component polyurethane structural adhesive can be mixed using a static mixing tube.
  • ? Coating operation
  • Use pneumatic or electric glue guns or other gluing equipment to apply ZJ-402 two-component polyurethane structural adhesive to the construction site.
  • matters needing attention:
  • When ZJ-402 two-component polyurethane structural adhesive is used in immersion applications, it should be fully cured before immersion;
  • Wet coating technology is not allowed, and it is recommended not to use solvents, water, cleaning agents, or soap solutions;
  • Before consulting the technical personnel of Zhijiang, it is not allowed to use high chlorine disinfection areas such as swimming pools.
  • Pre test procedure
  • In order to eliminate potential problems in the application site, Zhijiang can sample various materials used for adhesives, determine the best adhesive used in advance, and develop the best surface treatment method to obtain the best adhesive performance. Please consult the technical personnel of Zhijiang for specific information.
Color and packaging

According to customer requirements, we can provide 400 mL, 600 mL dual component rubber tube packaging or 20 L small barrels, 200 L large barrels packaging.

Storage and expiration date

It is recommended to store in a cool and dry place for a storage period of 6 months;

Incorrect storage conditions can affect product application and performance after curing.